MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCoat 8508-1 Heavy-Duty Epoxy Paint
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AboCoat 8508-1 is a heavy-duty epoxy paint. It excels as a protective and decorative coating for concrete, metal, wood, and composite surfaces, indoors and outdoors. It is applied to floors, walls, machinery, and installations in industrial, marine, and architectural environments. It is an excellent base coat for polyurethane and other coatings. Features: 2-component (1:1 ratio), solvent-based, superior adhesion, high-gloss, requires no primer, and available in standard and custom colors. Benefits: Corrosion inhibitor, even on rusty surfaces; Excellent for wear resistance in heavy-traffic areas and severe weather environments; Protects against water, weathering, fuels, and chemicals; Superior salt spray resistance; Can be applied to damp surfaces with excellent adhesion and film integrity; Can be used with sand and grit to make an anti-skid surface; Can be used for color-coding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 62 %
Volatile Organic Compounds (VOC) Content 220 g/lEPA method #24
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 1260 psiASTM-D4541
Coefficient of Friction 2.73Slip resistance; ASTM-D1894
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °CASTM-D2485
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 85.0 °FApplication Temperature
Shelf Life 24.0 Month
 
Descriptive Properties
Abrasive Resistance (g)0.088ASTM-D4060; CS 17/Load 1000/Cycles 1000
Chemical ResistanceHighASTM-D543
GlossHigh
Hardening Time (min)300-600
Impact Resistance72ASTM-D4226
Induction Period (min)10 to 15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics CHO-SHIELD® 610 A/B Conductive Epoxy Paint
Claude Bamberger Bamberko® 9016 Purge Compound
AISI Type A2 Tool Steel
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste

PABC836 / 107820

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.