Nylene NX 1170 HS is a high viscosity, heat stabilized grade formulated to give low wear properties through use of molybdenum disulfide at a high loading level. Testing conducted on dry as molded specimen at 73°F Information provided by Nylene® Global Polymer Solutions. |