MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LEXAN™ LUX2614G PC (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Developed for injection molding LED applications

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
 1.20 g/cc1.20 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.35 %0.35 %ASTM D570
 0.58 %
@Temperature 100 °C
0.58 %
@Temperature 212 °F
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
cm³/10 min; ISO 1133
 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 63.0 MPa9140 psi50 mm/min; ISO 527
 65.0 MPa9430 psi50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa8990 psi50 mm/min; ASTM D638
 63.0 MPa9140 psi50 mm/min; ISO 527
Elongation at Break 110 %110 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527
 7.0 %7.0 %50 mm/min; ASTM D638
Tensile Modulus 2.30 GPa334 ksi1mm/min; ISO 527
Flexural Yield Strength 93.0 MPa13500 psi1.3 mm/min, 50 mm span; ASTM D790
 94.0 MPa13600 psi2 mm/min; ISO 178
Flexural Modulus 2.30 GPa334 ksi2 mm/min; ISO 178
 2.34 GPa339 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 7.50 J/cm14.1 ft-lb/inASTM D256
Izod Impact, Unnotched 32.0 J/cm59.9 ft-lb/inASTM D4812
Tensile Impact Strength 546 kJ/m²260 ft-lb/in²ASTM D1822
Falling Dart Impact 169 J125 ft-lbASTM D3029
Taber Abrasion, mg/1000 Cycles 1010CS-17, 1 kg; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D257
Dielectric Constant  2.96
@Frequency 1e+6 Hz
2.96
@Frequency 1e+6 Hz
ASTM D150
 3.17
@Frequency 50.0 - 60.0 Hz
3.17
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 3.20 mm
381 kV/in
@Thickness 0.126 in
in air; ASTM D149
Dissipation Factor  0.00090
@Frequency 50.0 - 60.0 Hz
0.00090
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec15 - 30 secUL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs60 - 120 arcsUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831
Specific Heat Capacity 1.26 J/g-°C0.301 BTU/lb-°FASTM C 351
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°FASTM C177
Hot Ball Pressure Test 125 °C257 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
@Thickness 6.40 mm
279 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
@Thickness 6.40 mm
270 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 145 °C293 °FRate B/120; ISO 306
 154 °C309 °FRate B/50; ASTM D1525
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 V-2
@Thickness 0.750 - 1.65 mm
V-2
@Thickness 0.0295 - 0.0650 in
UL 94
Glow Wire Test  750 °C
@Thickness 0.750 mm
1380 °F
@Thickness 0.0295 in
IEC 60695-2-12
 850 °C
@Thickness 1.50 mm
1560 °F
@Thickness 0.0591 in
IEC 60695-2-12
 850 °C
@Thickness 1.50 mm
1560 °F
@Thickness 0.0591 in
IEC 60695-2-13
 875 °C
@Thickness 0.750 mm
1610 °F
@Thickness 0.0295 in
IEC 60695-2-13
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 305 - 325 °C581 - 617 °FInjection Molding
Zone 1 290 - 310 °C554 - 590 °F
Zone 2 300 - 320 °C572 - 608 °F
Zone 3 310 - 330 °C590 - 626 °F
Melt Temperature 310 - 330 °C590 - 626 °F
Mold Temperature 80.0 - 115 °C176 - 239 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10504 / 243971

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.