MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parker Chomerics CHO-SEAL 1485 Conductive Elastomer  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Conductive Elastomer EMI/EMP Gaskets

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 - 1.95 g/cc1.45 - 1.95 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 6555 - 65
Tensile Strength at Break >= 1.24 MPa>= 180 psiASTM D412
Elongation at Break >= 100 %>= 100 %ASTM D412
Tear Strength 5.25 kN/m30.0 pli
Compression Set 30 %
@Temperature 100 °C,
Time 252000 sec
30 %
@Temperature 212 °F,
Time 70.0 hour
ASTM D395 Method B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.020 ohm-cm0.020 ohm-cmas supplied without pressure sensitive adhesive
Shielding Effectiveness >= 50 dB>= 50 dB200 kHz (H Field); MIL-G-83528
 >= 80 dB>= 80 dB10 GHz (Plane Wave); MIL-G-83528
 >= 90 dB>= 90 dB2 GHz (Plane Wave); MIL-G-83528
 >= 100 dB>= 100 dB100 MHz (E Field); MIL-G-83528
 >= 100 dB>= 100 dB500 MHz (E Field); MIL-G-83528
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 85.0 °C185 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
BinderSilicone
EMP Survivability kA / in, min0.3
FillerAg/Al
Heat Aging ohm-cm max0.06
Vibration Resistance, After, ohm-cm max0.02
Vibration Resistance, During, ohm-cm max0.06

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer
Parker Chomerics CHO-SEAL 1239 Conductive Elastomer
Parker Chomerics CHO-SEAL 1224 Conductive Elastomer
Parker Chomerics CHO-SEAL 1215 Conductive Elastomer
Parker Chomerics CHO-SEAL 1212 Conductive Elastomer

PCHOME111 / 28333

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.