MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Medalist® MD-23173 Thermoplastic Vulcanizate Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Medalist MD-23173 is a high performance thermoplastic vulcanizate specifically designed for healthcare and medical applications. Medalist MD-23173 is a high hardness, low density, RoHS compliant grade that can be sterilized grade suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability; Good Flexibility; Good Moldability; Good Sterilizability; Good Tear Strength; Good Toughness; Halogen Free; Low Density; High Hardness; Low Specific Gravity; Radiation Sterilizable; Resilient

Uses: Dental Applications; Gaskets; Hospital Goods; Medical Devices; Medical/Healthcare Applications; Pharmaceuticals; Plugs; Rubber Replacement; Seals

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D792
Melt Flow 24 g/10 min
@Load 5.00 kg,
Temperature 200 °C
24 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  73
@Time 5.00 sec
73
@Time 0.00139 hour
Injection Molded; ASTM D2240
 75
@Time 1.00 sec
75
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 7.10 MPa1030 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain  4.12 MPa
@Strain 100 %
598 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 6.16 MPa
@Strain 300 %
894 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 390 %390 %Die C, 20 in/min; ASTM D412
Tear Strength 36.1 kN/m206 pliDie C, 20 in/min; ASTM D624
Compression Set  27 %
@Temperature 22.8 °C,
Time 79200 sec
27 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 46 %
@Temperature 70.0 °C,
Time 79200 sec
46 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 52 %
@Temperature 100 °C,
Time 79200 sec
52 %
@Temperature 212 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 149 - 171 °C300 - 340 °F
Middle Barrel Temperature 171 - 193 °C340 - 380 °F
Front Barrel Temperature 193 - 216 °C380 - 420 °F
Nozzle Temperature 193 - 216 °C380 - 420 °F
Melt Temperature 193 - 216 °C380 - 420 °F
Mold Temperature 15.6 - 37.8 °C60.0 - 100 °F
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0718 / 237209

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.