MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Hipscon™ M-505 Static Control High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Hipscon™ M-505 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are lightweight and easily formed into deep pockets that maintain uniform static protection. Hipscon maintains extremely low gloss surfaces after forming, allowing for easy reading of package contents via automated sensors. Hipscon™ M-505 sheet is available in custom extruded gauges from 0.012 to 0.080 inch and widths of 10 to 48 inches. Product is typically provided as rollstock with a smooth surface finish.

Features:

  • Hipscon M-505 Chloride free(<0.3 ppm), M-505 will not corrode sensitive metal leads
  • Low chloride levels
  • High degree stiffness
  • Low gloss
  • Superior impact strength

Applications:

  • Disk drive packaging
  • Electronic component handling
  • Electronic component packaging

Data provided by Noveon, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2600 psiASTM D638
Elongation at Break 1.3 %ASTM D638
Flexural Modulus 230000 psiASTM D790-92
Tear Strength 68.0 kN/mASTM D646
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+7 ohm-cmASTM D257
Surface Resistivity per Square 1e+0550% RH; ASTM D257
Static Decay <= 0.010 secFTMS-101C; 12% R.H., (+5000 V to 50 V)
 <= 0.010 secFTMS-101C; 12% R.H., (-5000 V to -50 V)
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Gloss 9.0 %60°; Front
 14 %60°; Back
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tabriz WT1235 High Impact Polystyrene
Total Impact Polystyrene 940E Super High Impact Polystyrene, Sheet Extrusion and Thermoforming Grade
Americas Styrenics STYRON® EA6740 High Impact Polystyrene
Americas Styrenics Styron® 425 High Impact Polystyrene
Americas Styrenics STYRON® 404 High Impact Polystyrene

PNOVEON02 / 55285

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.