MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® Easy Slide I PEEK, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: VESTAKEEP® Easy Slide I is a carbon fiber-reinforced, wear and friction modified polyether ether ketone for injection molding. The semi-crystalline polymer features superior, thermal and chemical resistance. Parts made from VESTAKEEP® Easy Slide I are flame resistant and can be used for bearing bushing or gearbox parts due to the self-lubricating effect. VESTAKEEP® Easy Slide I can be processed by common machines for thermoplastics. The manufacturer recommends a melt temperature between 380°C and 400°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C. VESTAKEEP® Easy Slide I is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. For information about processing of VESTAKEEP® Easy Slide I, please follow the general recommendations in our brochure “VESTAKEEP® PEEK Processing Recommendations“. Pigmentation may affect values.
Dry properties listed below
Industrial Sector: Industry and Engineering
Processing: Injection molding
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Fire / burn
Additives: Carbon fibers
Applications: Electrical and Electronical, Encapsulation
Special Characteristics: Semi-crystalline
Features: High coefficient of friction
Color: Natural color
Chemical Resistance: General chemical resistance

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.00300 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00700 cm/cmISO 294-4, 2577
Melt Flow 20.0 g/10 min
@Load 5.00 kg,
Temperature 380 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 160 MPaISO 527
Elongation at Break 2.00 %Nominal; ISO 527
Tensile Modulus 12000 MPaISO 527
Charpy Impact, Notched 5.50 kJ/m²Type of failure: C; ISO 179/1eA
Coefficient of Friction 0.210parallel; ISO 7148-2
 0.240normal; ISO 7148-2
K (wear) Factor 0.0240 x 10-8 mm³/N-M
@Pressure 4.00 MPa
normal, test speed: 0.5 m/s; ISO 7148-2
 0.0380 x 10-8 mm³/N-M
@Pressure 4.00 MPa
parallel, test speed: 0.5 m/s; ISO 7148-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1e+05?V; IEC 62631-3-1
Surface Resistance 1e+05RDS; IEC 62631-3-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 340 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 338 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 321 °CISO 75-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 °CInjection Molding; ISO 294
 380 °C
Mold Temperature 180 °CInjection Molding; ISO 294
 180 °C
Injection Velocity 200 mm/secInjection Molding; ISO 294
Moisture Content 0.0600 %ISO 15512
 
Descriptive Properties
ColorNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7860 / 324992

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.