MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Zortrax Z-ULTRAT Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Z-ULTRAT is a material characterized by high impact resistance, which gives your models a uniform surface texture. This all-purpose material allows you to 3D print elements requiring durability, such as end-use parts, which, after continued use, keep their initial shape over time. With Z-ULTRAT, you can produce objects with properties comparable to those of models manufactured using injection molding technology, including functional prototypes, test casings, and mechanical parts. Z-ULTRAT allows you to test your tailor-made projects in unlimited ways, in one of twenty-two shades.

Information provided by Zortrax

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.179 g/cc0.04259 lb/in³ISO 1183-3:2003
Melt Flow 43.88 g/10 min
@Load 5.00 kg,
Temperature 260 °C
43.88 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133:2006
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 73.473.4ISO 868:1998
Tensile Strength at Break 30.7 MPa4450 psiISO 527:1998
Tensile Strength 32.6 MPa4730 psiISO 527:1998
Elongation at Break 4.87 %4.87 %ISO 527:1998
Elongation at Yield 3.78 %3.78 %ISO 527:1998
Flexural Strength 54.0 MPa7830 psiISO 178:2011
Flexural Modulus 1.85 GPa268 ksiISO 178:2011
Izod Impact, Notched (ISO) 5.26 kJ/m²2.50 ft-lb/in²ISO 180:2004
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 106.4 °C223.5 °FISO 11357-3:2014

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZORT011 / 281890

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.