MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Primex Plastics Prime ABS 750 Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Prime ABS 750 is a general purpose ABS product that has good impact strength, and good hot strength for thermoforming. It is an amorphous thermoplastic material and therefore, processes easier than some other thermoplastic materials.

Applications: Prime ABS 750 may be used for interior applications such as appliance parts, tub and shower wall surrounds, and interior automotive trim. With the addition of a weatherable cap it may also be used in many outdoor applications.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Melt Flow 1.7 g/10 min1.7 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102102ASTM D785
Tensile Strength, Yield 35.2 MPa5100 psiASTM D638
Flexural Strength 55.2 MPa8000 psiASTM D790
Flexural Modulus 1.86 GPa270 ksiASTM D790
Izod Impact, Notched  1.17 J/cm
@Temperature -40.0 °C
2.20 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 3.36 J/cm
@Temperature 22.8 °C
6.30 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C198 °FASTM D648
Vicat Softening Point 107 °C224 °FASTM D1525
Flammability, UL94 HB
@Thickness >=1.52 mm
HB
@Thickness >=0.0600 in
 
Optical PropertiesMetricEnglishComments
Gloss 90 %90 %60° Angle; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRIM000 / 278471

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.