MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Meyors Chemical HD 60-33S Rubber Vulcanization Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Code: MSHQD -VA030-03 OT
Chemical Name: Polymeric Sulfur
Trade Name: Rubber Vulcanization agent HD 60-33S
CAS No.: Polymeric Sulfur: 9035-99-8; Rhombic Sulfur: 7704-34-9; Silicon dioxide: 7631-86-9; High pressure and hydrotreated naphthenic oil: 64742-52-5

Typical Properties: Yellow powder with slight odor, non-toxic. HD 60-33S is not stable and can convert to soluble sulfur. HD 60-33S is insoluble in CS2 and in water.

Recommended Applications: Because insoluble sulfur is metastable temperature should be kept as low as possible during mixing. Between 100-130°C significant reversions can take place to soluble sulfur. Insoluble sulfur reversion can take place if it is in direct contact with alkaline components. Due to the optimal dispersion during mixing stage, it seldom appears electrostatic charge accumulating and form agglomerates

Information provided by Meyors Chemical INC Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 - 1.60 g/cc0.0542 - 0.0578 lb/in³
Molecular Weight 256.5 g/mol256.5 g/mol
Ash <= 8.5 %<= 8.5 %with 8% Silica
 
Descriptive Properties
AppearanceNon-rised yellow powder
Content<0.05%Acidity(as H2S04)
 <0.5%Residues ( 63µm)
 >90%Insoluble sulfur content (On total S)
 24-26%Oil
 66-68%Element Sulfur
Loss on drying<0.5%
Stability>80%high temperature (105 ?15 minutes) insoluble sulfur content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMEYORS039 / 316621

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.