MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin NH5020 Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ NH5020 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and exhibits high heat resistance with thin-wall FR performance. NORYL NH5020 resin carries a UL94 flame rating of V0 at 0.75mm along with a UL746C Outdoor Suitability rating of F1. The material offers a good balance of affordable high heat, flow, hydrolytic stability, excellent creep resistance, dimensional stability and is a good candidate for photovoltaic / solar connectors, UPS Inverters / chargers, and outdoor enclosure applications.

Features: Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0500 %0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %0.25 %ISO 62-1
Viscosity 10 cP
@Load 5.00 kg,
Temperature 280 °C
10 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 9.8 g/10 min
@Load 5.00 kg,
Temperature 280 °C
9.8 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.0 MPa8990 psi50 mm/min; ASTM D638
 77.0 MPa11200 psi50 mm/min; ISO 527
Tensile Strength, Yield 79.0 MPa11500 psi50 mm/min; ASTM D638
 80.0 MPa11600 psi50 mm/min; ISO 527
Elongation at Break 5.6 %5.6 %50 mm/min; ISO 527
 15 %15 %50 mm/min; ASTM D638
Elongation at Yield 4.7 %4.7 %50 mm/min; ISO 527
 5.0 %5.0 %50 mm/min; ASTM D638
Tensile Modulus 2.72 GPa395 ksi50 mm/min; ASTM D638
 3.05 GPa442 ksi1 mm/min; ISO 527
Flexural Strength 122 MPa17700 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 126 MPa18300 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.98 GPa432 ksi2 mm/min; ISO 178
 3.00 GPa435 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 91.0 J67.1 ft-lbASTM D256
 59.0 J
@Temperature -30.0 °C
43.5 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 19.0 J14.0 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 49.0 kV/mm
@Thickness 3.20 mm
1240 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  61.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 61.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  68.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 68.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)  122 °C
@Thickness 3.20 mm
252 °F
@Thickness 0.126 in
unannealed; ASTM D648
 133 °C
@Thickness 6.40 mm
271 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 119 °C246 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 117 °C
@Thickness 3.20 mm
243 °F
@Thickness 0.126 in
unannealed; ASTM D648
 122 °C
@Thickness 6.40 mm
252 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 137 °C279 °FRate B/50; ASTM D1525
 138 °C280 °FRate B/50; ISO 306
 139 °C282 °FRate B/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 275 - 305 °C527 - 581 °F
Zone 2 255 - 300 °C491 - 572 °F
Zone 3 265 - 305 °C509 - 581 °F
Melt Temperature 275 - 305 °C527 - 581 °FInjection Molding
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 105 - 110 °C221 - 230 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82385 / 290332

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.