MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL GTX™ Resin GTX918W Polyphenylene Ether + PA (PPE+Nylon) (Americas)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 918W resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits high heat resistance, excellent chemical resistance, and high melt flow. NORYL GTX918W resin may be an excellent candidate for automotive under-the-hood and electrical applications requiring the retention of properties while under thermal load.

Features: Hydrolytic Stability,Low Creep Sensitivity,Good Stiffness,Low Warpage,High Flow,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Moisture Absorption 0.0700 %0.0700 %Injection Molding
Linear Mold Shrinkage, Flow 0.013 - 0.016 cm/cm
@Thickness 3.20 mm
0.013 - 0.016 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.010 - 0.013 cm/cm
@Thickness 3.20 mm
0.010 - 0.013 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 62.0 MPa8990 psi50 mm/min; ASTM D638
Elongation at Break 53 %53 %50 mm/min; ASTM D638
Flexural Strength 98.0 MPa14200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.36 GPa342 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 202 J149 ft-lbASTM D256
Dart Drop, Total Energy 40.0 J29.5 ft-lbpeak; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 188 °C
@Thickness 3.20 mm
370 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 148 °C
@Thickness 3.20 mm
298 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 270 - 295 °C518 - 563 °F
Zone 2 260 - 295 °C500 - 563 °F
Zone 3 265 - 295 °C509 - 563 °F
Melt Temperature 270 - 295 °C518 - 563 °FInjection Molding
Mold Temperature 65.0 - 95.0 °C149 - 203 °F
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %minimum
Back Pressure 0.300 - 1.40 MPa43.5 - 203 psi
Shot Size 30 - 50 %30 - 50 %
Vent Depth 0.00130 - 0.00380 cm0.000512 - 0.00150 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82166 / 290113

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.