MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lyanchemicals Tech DINP
Categories: Other Engineering Material

Material Notes: Introduction:Diisononyl phthalate (DINP) is produced by esterifying lsononanol and Phthalic anhydride. DINP 's plasticizing characteristic is similar to that of DEHP. However, DINP's low volatilty is advantageous for certain applications. DINP is a general plasticizer. Compared to DEHP, DINP's plasticizing efficiency, migration and water extraction rate are lower, while its gelation temperature and electric resistivity are mily higher. DINP s low volatilty not only extends the life of a product, but also reduces volatility during processing.

Information provided by Lyanchemicals Tech Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.975 - 0.981 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.050[mg KOH/g]
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 3.00e+11 ohm-cm
@Temperature 30.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.481 - 1.487
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %
 
Descriptive Properties
Color<25APHA
ContentEster
Heat Loss<0.1%122-128°C x 3hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLYANT014 / 318041

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.