MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay MIRACARE® PLAISANT Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Description: This is a plant-based system for cleansing cosmetics. Ultra mild, with excellent foam volume and lather characteristics, it is compatible with anionic, nonionic and amphoteric surfactants allowing the flexibility to develop environment friendly and sulfate-free formulations. It can be used as a primary base, or simply as a performance enhancer additive and is perfectly suitable for men's shower gel and shampoo, body wash, conditioning shampoo and facial wash.

Chemical Name: SURFACTANT BLEND

INCI Listing: Water, Sodium Cocoyl Isethionate, Sodium Lauroamphoacetate, Sodium Methyl Cocoyl Taurate

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRACARE© PLAISANT is a plant-based system for cleansing cosmetics. Ultra mild, with excellent foam volume and lather characteristics, it is compatible with anionic, nonionic and amphoteric surfactants allowing the flexibility to develop environment-friendly and sulfate-free formulations. MIRACARE© PLAISANT is easy to handle and formulate with. Simply dilute in water, and include desired additives such as polymers, surfactants, pearlizers, dyes, fragrances, and preservatives. MIRACARE© PLAISANT is a natural and gentle ingredient that can be used as a primary base, or simply as a performance enhancer additive. It is perfectly suited for: Men’s shower gel and shampoo; Body wash; Conditioning shampoo; Facial wash; and Liquid hand soap. The recommended use levels are from 5 to 20% when used as a performance additive, and up to 60% when used as the primary ingredient.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 35 - 38 %
@Temperature 105 °C,
Time 7200 sec
35 - 38 %
@Temperature 221 °F,
Time 2.00 hour
Oven; RP-0540
pH 7.5 - 8.57.5 - 8.5RP-0420
Viscosity <= 7500 cP<= 7500 cP#4 SP @ 10 rpm; RP-0659
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 3.0
@Temperature 35.0 °C
<= 3.0
@Temperature 95.0 °F
RP-0138
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceOpaque LiquidSeparates on Standing, RP-0064
Composition2-Methyl-4-Isothiazolon-3-One60-80 ppm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD247 / 137478

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.