MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik Sanicro 56 Tube and Pipe, Seamless (UNS N10276)
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Sanicro 56 (UNS N10276) is a nickel-chromium-molybdenum alloy suitable for service in a broad range of severe environments and is characterized by:
  • Superior corrosion resistance in H2S, CO2 and chloride containing environments
  • Excellent resistance to pitting corrosion owing to its high PRE value of 68
  • Excellent corrosion resistance in hydrochloric acid
The grade is suitable for use in a number of severe industrial environments, such as mixed acid chemical processing, pulp and paper production, industrial and municipal waste treatment and oil and gas.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 690 MPa>= 100000 psiRm
Tensile Strength, Yield >= 283 MPa
@Strain 0.2 %
>= 41000 psi
@Strain 0.2 %
Elongation at Break >= 40 %>= 40 %
Modulus of Elasticity  159 GPa
@Temperature 800 °C
23100 ksi
@Temperature 1470 °F
 167 GPa
@Temperature 700 °C
24200 ksi
@Temperature 1290 °F
 178 GPa
@Temperature 600 °C
25800 ksi
@Temperature 1110 °F
 180 GPa
@Temperature 500 °C
26100 ksi
@Temperature 932 °F
 192 GPa
@Temperature 300 °C
27800 ksi
@Temperature 572 °F
 198 GPa
@Temperature 200 °C
28700 ksi
@Temperature 392 °F
 203 GPa
@Temperature 100 °C
29400 ksi
@Temperature 212 °F
 205 GPa
@Temperature 25.0 °C
29700 ksi
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.2 µm/m-°C
@Temperature 25.0 - 100 °C
6.78 µin/in-°F
@Temperature 77.0 - 212 °F
 12.4 µm/m-°C
@Temperature 25.0 - 200 °C
6.89 µin/in-°F
@Temperature 77.0 - 392 °F
 12.9 µm/m-°C
@Temperature 25.0 - 300 °C
7.17 µin/in-°F
@Temperature 77.0 - 572 °F
 13.2 µm/m-°C
@Temperature 25.0 - 400 °C
7.33 µin/in-°F
@Temperature 77.0 - 752 °F
 13.5 µm/m-°C
@Temperature 25.0 - 500 °C
7.50 µin/in-°F
@Temperature 77.0 - 932 °F
 13.6 µm/m-°C
@Temperature 25.0 - 600 °C
7.56 µin/in-°F
@Temperature 77.0 - 1110 °F
 14.1 µm/m-°C
@Temperature 25.0 - 700 °C
7.83 µin/in-°F
@Temperature 77.0 - 1290 °F
 14.8 µm/m-°C
@Temperature 25.0 - 800 °C
8.22 µin/in-°F
@Temperature 77.0 - 1470 °F
Specific Heat Capacity 0.427 J/g-°C0.102 BTU/lb-°F
Thermal Conductivity  7.20 W/m-K
@Temperature -168 °C
50.0 BTU-in/hr-ft²-°F
@Temperature -270 °F
 8.70 W/m-K
@Temperature -73.0 °C
60.4 BTU-in/hr-ft²-°F
@Temperature -99.4 °F
 9.80 W/m-K
@Temperature 20.0 °C
68.0 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 11.2 W/m-K
@Temperature 100 °C
77.7 BTU-in/hr-ft²-°F
@Temperature 212 °F
 14.7 W/m-K
@Temperature 300 °C
102 BTU-in/hr-ft²-°F
@Temperature 572 °F
 20.0 W/m-K
@Temperature 600 °C
139 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 25.4 W/m-K
@Temperature 900 °C
176 BTU-in/hr-ft²-°F
@Temperature 1650 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.010 %<= 0.010 %
Chromium, Cr 16 %16 %
Cobalt, Co <= 2.5 %<= 2.5 %
Iron, Fe 4.5 %4.5 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 16 %16 %
Nickel, Ni 57 %57 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.080 %<= 0.080 %
Sulfur, S <= 0.015 %<= 0.015 %
Tungsten, W 3.5 %3.5 %
Vanadium, V <= 0.35 %<= 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy C-276
ATI Allvac® Nickelvac® C-276 UNS N10276 Nickel Superalloy
Sandvik Sanicro 56 Covered electrodes (UNS N10276)
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276
Carlson GOC 276 Nickel-Molybdenum-Chromium

NSANDV5302 / 199866

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.