Description: - Flexible, low density, high loss, carbon impregnated foam dielectric absorber with PSA and Mylar.
- Construction: Bottom Layer: PSA; Middle Layer: Foam; Top Layer: Mylar
- Ideal for applications requiring absorption across a wide range of frequencies, including antenna cross-talk and side lobe reduction and cavity resonance suppression.
- RoHS and REACH compliant.
Information provided by Hexcel Corporation. |