MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Smooth-Cast® 320 Off-White, Ultra Low Viscosity Liquid Plastics
Categories: Polymer; Thermoplastic

Material Notes: Product Overview: The Smooth-Cast™ 320 Series consists of ultra-low viscosity casting resins that yield virtually bubble-free off-white castings. The Smooth-Cast™ 320 resins are sister products to our popular Smooth-Cast™ 300 Series of bright white plastics, but are easier to color using SO-Strong™, UVO™ or Ignite™ color tints. Smooth-Cast™ 320 series is easy to mix and pour, offering the convenience of a 1A:1B by volume or 100A : 90B by weight mix ratio. The Smooth-Cast™ 320 Series resins readily accept pigments and fillers (such as URE-FIL™ 3, 5 and 7 from Smooth-On). Fully cured castings are tough, durable, machinable and paintable. They resist moisture and mild solvents. Applications for Smooth-Cast™ 320 Series resins include reproducing small to medium size sculptures, making prototype models, special effect props, decorative jewelry and taxidermy (bones, antlers, teeth etc.).

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D-1475
Viscosity 80 cP80 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ASTM D-2240
Tensile Strength, Ultimate 20.7 MPa3000 psiASTM D-638
Elongation at Break 10 %10 %ASTM D-638
Tensile Modulus 0.951 GPa138 ksiASTM D-638
Flexural Strength 31.0 MPa4500 psiASTM D-790
Flexural Modulus 0.910 GPa132 ksiASTM D-790
Compressive Strength 25.2 MPa3650 psiASTM D-695
Compressive Modulus 0.316 GPa45.8 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 60.0 °C140 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hourHandling Time
Pot Life 3.00 min3.00 minASTM D-2471
 
Descriptive Properties
ColorOff-White
Mix Ratio100A:90Bby weight
 1A:1Bby volume
Specific Volume26.4[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN019 / 296720

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.