MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient OnFlex™ BIO 5380A-E0006 Thermoplastic Elastomer (TPE)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™ BIO 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable material as certified according to ASTM-D6866. The OnFlex™ BIO 5300 series compounds are formulated to provide an excellent surface finish, soft-touch haptic, abrasion resistance and mechanical properties.

Properties are measured using injection molded plaques.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ISO 868
Tensile Strength at Break  19.8 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
2870 psi
@Thickness 0.0787 in,
Temperature 73.4 °F
Type 1, 200 mm/min; Flow; DIN 53504
 20.0 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
2900 psi
@Thickness 0.0787 in,
Temperature 73.4 °F
Type 1, 200 mm/min Across Flow; DIN 53504
Tensile Stress at Strain  4.40 MPa
@Strain 100 %,
Thickness 2.00 mm
638 psi
@Strain 100 %,
Thickness 0.0787 in
Type 1, 200 mm/min Across Flow; DIN 53504
 4.50 MPa
@Strain 100 %,
Thickness 2.00 mm
653 psi
@Strain 100 %,
Thickness 0.0787 in
Type 1, 200 mm/min; Flow; DIN 53504
 10.0 MPa
@Strain 300 %,
Thickness 2.00 mm
1450 psi
@Strain 300 %,
Thickness 0.0787 in
Type 1, 200 mm/min Across Flow; DIN 53504
 10.2 MPa
@Strain 300 %,
Thickness 2.00 mm
1480 psi
@Strain 300 %,
Thickness 0.0787 in
Type 1, 200 mm/min; Flow; DIN 53504
Elongation at Break  500 %
@Thickness 2.00 mm,
Temperature 23.0 °C
500 %
@Thickness 0.0787 in,
Temperature 73.4 °F
Type 1, 200 mm/min; Flow; DIN 53504
 520 %
@Thickness 2.00 mm,
Temperature 23.0 °C
520 %
@Thickness 0.0787 in,
Temperature 73.4 °F
Type 1, 200 mm/min Across Flow; DIN 53504
Tear Strength  64.0 kN/m
@Thickness 2.00 mm,
Temperature 23.0 °C
365 pli
@Thickness 0.0787 in,
Temperature 73.4 °F
Method A, Trouser; Across Flow; ISO 34-1
 64.0 kN/m
@Thickness 2.00 mm,
Temperature 23.0 °C
365 pli
@Thickness 0.0787 in,
Temperature 73.4 °F
Method A, Trouser; Flow; ISO 34-1
Abrasion 3838[mm³]; DIN 53516
Compression Set  47 %
@Temperature 23.0 °C,
Time 259000 sec
47 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 71 %
@Temperature 70.0 °C,
Time 79200 sec
71 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 84 %
@Temperature 100 °C,
Time 79200 sec
84 %
@Temperature 212 °F,
Time 22.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 220 °C356 - 428 °F
Mold Temperature 30.0 - 60.0 °C86.0 - 140 °F
Drying Temperature 100 - 120 °C212 - 248 °F
Dry Time 1.00 - 2.00 hour1.00 - 2.00 hour
 
Descriptive Properties
FeaturesGood Abrasion Resistance
 Renewable Resource Content
 Scratch Resistant
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Injection RateFast
Odor rating3.2VDA 270; Method A3
Processing MethodCalendering
 Extrusion
 Injection Molding
 Multi Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAutomotive Applications
 Consumer Applications
 General Purpose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Avient OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE)
Avient OnFlex™ U 5370A-S0015 Thermoplastic Elastomer (TPE)
Avient OnFlex™ U 5380A-S0013 Thermoplastic Elastomer (TPE)
Avient OnFlex™ U 5470A-E0083 Thermoplastic Elastomer (TPE)

PH0POL1031 / 145600

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.