MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Vinnolit® E 2169 Emulsion PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vinnolit® E 2169 Emulsion PVC for thermoplastic processing of PVC. Vinnolit® E 2169 is an emulsion polymer primarily used to make semi-rigid and flexible profiles and films as well as flooring. Vinnolit® E 2169 serves as the main component or blend component for making PVC compounds with the usual additives by standard mixing techniques. Mixtures containing Vinnolit® E 2169 are preferably processed to semi-rigid and flexible tubing, profiles and film. Vinnolit® E 4069 is also an excellent blend component for flooring formulations. Vinnolit® E 2169 accelerates fusion and improves melt homogeneity. Mixtures containing Vinnolit® E 2169 are thus very easy to process. The product also contributes to the antistatic properties of the finished parts.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.50 %<= 0.50 %ISO 1269
Apparent Bulk Density 0.560 g/cc0.0202 lb/in³ISO 60
Particle Size <= 250 µm<= 250 µm<= 0.1% Retained on 0.25 mm Sieve; ISO 4610
Viscosity Test 120 cm³/g1.2 dl/gReduced Viscosity; ISO 1628-2
 
Descriptive Properties
K-Value69ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVINNO916 / 291113

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.