MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Superwool® Paper 351-E Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: AES Fiber Class. Expandable fiber grade. Superwool 351-E expandable paper is an intumescent material produced from a unique blend of Superwool bulk fibers, special additives, and organic binders. At maximum expansion which occurs at approximately 1200°F (649°C), the paper expands up to 400% of its thickness. This results in the 351-E paper being an excellent candidate for high temperature gaskets and seals, and fire protection applications. During heat up and expansion, there will be some additional outgassing of the intumescent additives.

Applications:

  • All-purpose high temperature gasketing and sealing
  • Fire protection
  • Fire doors
  • Expansion joint insulation
  • Fireplace catalytic converter gasketing
  • Aluminum filter bowl gasketing

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.240 - 0.288 g/cc0.00867 - 0.0104 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.0300 - 0.0700 MPa4.35 - 10.2 psifired
 0.520 - 0.690 MPa75.4 - 100 psi
 
Thermal PropertiesMetricEnglishComments
Melting Point 1275 °C2327 °F
Maximum Service Temperature, Air 1000 °C1830 °FContinuous Use
 
Component Elements PropertiesMetricEnglishComments
CaO+MgO 23 - 37 %23 - 37 %after firing
Carbon, C 5.0 - 10 %5.0 - 10 %after firing
Other 6.0 - 10 %6.0 - 10 %organic binder
SiO2 55 - 65 %55 - 65 %after firing
 
Descriptive Properties
Classification Temperature (°C)1100
Colorgray
Expansion Ratio (%)3583.17mm thick, at 981°C
 4143.17 mm thick, at 790°C
 4193.17mm thick, at 540°C
 863.17mm thick, at 204°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Morgan Advanced Ceramics Ceraform 250 Ceramic Fiber
Morgan Advanced Ceramics Cerafibre® Bulk Thermal Ceramic
Morgan Advanced Ceramics Cerafiber® Refractory Ceramic Fiber Bulks Thermal Ceramic
Morgan Advanced Ceramics Cerachrome® Refractory Ceramic Fiber Bulks Thermal Ceramic

CMORF70125 / 203423

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.