MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NYCOA NY-FLEX® CT 176 Nylon-Based TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Nylon (Polyamide PA)

Material Notes: NY-FLEX® E-TPE grades deliver excellent flexibility at low temperature, superior retention of properties to elevated temperature, exceptional impact toughness and resilience. These also exhibit high creep resistance, strong resistance to flex fatigue, good abrasion resistance, and good resistance to greases, oils, and solvents.

These materials are block copolymers of nylon (polyamide) segments and polyether segments. Physical properties vary with the ratio of the two components.

'Dry' samples tested as-molded - <0.3% moisture. 'Conditioned' samples are equilibrated at 50% RH and 23°C.

Information provided by Nylon Corporation of America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792
Water Absorption 3.5 %
@Time 86400 sec
3.5 %
@Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 2.6 %2.6 %50% RH; ASTM D570
Linear Mold Shrinkage 0.011 - 0.014 cm/cm0.011 - 0.014 in/inNYCOA Test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  70
@Time 15.0 sec
70
@Time 0.00417 hour
Conditioned; ASTM D2240
 74
@Time 0.000 sec
74
@Time 0.000 hour
Conditioned; ASTM D2240
 74
@Time 15.0 sec
74
@Time 0.00417 hour
Dry; ASTM D2240
 76
@Time 0.000 sec
76
@Time 0.000 hour
Dry; ASTM D2240
Tensile Strength 42.0 MPa6090 psiConditioned; ASTM D638
 50.0 MPa7250 psiDry; ASTM D638
Tensile Stress at Strain  18.0 MPa
@Strain 5.0 %
2610 psi
@Strain 5.0 %
Conditioned; ASTM D638
 26.0 MPa
@Strain 10 %
3770 psi
@Strain 10 %
Conditioned; ASTM D638
 29.0 MPa
@Strain 50 %
4210 psi
@Strain 50 %
Conditioned; ASTM D638
 38.0 MPa
@Strain 5.0 %
5510 psi
@Strain 5.0 %
Dry; ASTM D638
 38.0 MPa
@Strain 50 %
5510 psi
@Strain 50 %
Dry; ASTM D638
 42.0 MPa
@Strain 10 %
6090 psi
@Strain 10 %
Dry; ASTM D638
Elongation at Break >= 250 %>= 250 %Dry; ASTM D638
 >= 250 %>= 250 %Conditioned; ASTM D638
Tensile Modulus 0.620 GPa89.9 ksiConditioned; ASTM D638
 1.20 GPa174 ksiDry; ASTM D638
Flexural Strength 23.0 MPa3340 psiConditioned; ASTM D790
 35.0 MPa5080 psiDry; ASTM D790
Flexural Modulus 0.520 GPa75.4 ksiConditioned; ASTM D790
 1.275 GPa184.9 ksiDry; ASTM D790
Izod Impact, Notched  0.750 J/cm
@Temperature -30.0 °C
1.41 ft-lb/in
@Temperature -22.0 °F
Dry; ASTM D256
 0.850 J/cm
@Temperature -30.0 °C
1.59 ft-lb/in
@Temperature -22.0 °F
Conditioned; ASTM D256
 1.60 J/cm
@Temperature 23.0 °C
3.00 ft-lb/in
@Temperature 73.4 °F
Dry; ASTM D256
 3.42 J/cm
@Temperature 23.0 °C
6.41 ft-lb/in
@Temperature 73.4 °F
Conditioned; ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ASTM D256
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ASTM D256
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ASTM D256
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 213 °C415 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NYCOA NY-FLEX® CT 145 Nylon-Based TPE
NYCOA NY-FLEX® CT 155 Nylon-Based TPE
NYCOA NY-FLEX® CT 164 Nylon-Based TPE
NYCOA NY-FLEX® CT 172 Nylon-Based TPE
NYCOA NY-FLEX® CT 180 Nylon-Based TPE

PNYCOA91 / 217539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.