MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Rolled Zinc Alloy (Zn-1.0Cu-0.010Mg), Cold-Rolled - Longitudinal Properties
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Hot Work Temperature 175-300°C

Properties vary with rolling direction. Average values and values for transverse direction are listed separately.

Key Words: UNS Z45330
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.17 g/cc0.259 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8080500 kg load; 10 mm hardened steel ball
Hardness, Knoop 103103Estimated from Brinell Value
Hardness, Rockwell B 4949Estimated from Brinell Value
Hardness, Vickers 9090Estimated from Brinell Value
Tensile Strength, Ultimate 248 MPa36000 psi
Elongation at Break 25 %25 %in 5 cm
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000620 ohm-cm0.00000620 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 34.8 µm/m-°C
@Temperature 20.0 °C
19.3 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.401 J/g-°C0.0958 BTU/lb-°F
Thermal Conductivity 105 W/m-K729 BTU-in/hr-ft²-°F
Melting Point 419 - 422 °C786 - 792 °F
Solidus 419 °C786 °F
Liquidus 422 °C792 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 175 °C347 °F
Hot-Working Temperature 175 - 300 °C347 - 572 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0010 %<= 0.0010 %
Cadmium, Cd <= 0.040 %<= 0.040 %
Copper, Cu 0.85 - 1.25 %0.85 - 1.25 %
Iron, Fe <= 0.015 %<= 0.015 %
Lead, Pb <= 0.15 %<= 0.15 %
Magnesium, Mg 0.0060 - 0.016 %0.0060 - 0.016 %
Tin, Sn <= 0.0010 %<= 0.0010 %
Zinc, Zn 98.527 - 99.144 %98.527 - 99.144 %As balance; per ASTM B 69

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Commercial Rolled Zinc (Zn-0.06Pb-0.06Cd), Hot-Rolled - Longitudinal Properties
Rolled Zinc Alloy (Zn-1.0Cu-0.010Mg), Cold-Rolled - Transverse Properties
Rolled Zinc Alloy (Zn-1.0Cu-0.010Mg), Hot-Rolled - Longitudinal Properties
Rolled Zinc Alloy (Zn-1.0Cu-0.010Mg), Hot-Rolled - Transverse Properties
Commercial Rolled Zinc (Zn-0.06Pb-0.06Cd), Hot-Rolled - Transverse Properties

MZN652 / 14537

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.