MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Toyobo Riteflex® 672A Thermoplastic Copolyester Elastomer
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Product Description: Riteflex 672A is a 72 Shore D Hardness thermoplastic polyester elastomer with a high modulus.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Maximum Moisture Content 0.0500.050
Linear Mold Shrinkage 0.017 - 0.022 cm/cm0.017 - 0.022 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.017 - 0.020 cm/cm0.017 - 0.020 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 22.0 MPa3190 psiISO 527-2/50
Elongation at Break >= 50 %>= 50 %Nominal; ISO 527-2/50
Charpy Impact, Notched  0.504 J/cm²
@Temperature -30.0 °C
2.40 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.89 J/cm²
@Temperature 22.8 °C
9.00 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 215 °C419 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FUnannealed; ISO 75-2/B
Vicat Softening Point 205 °C401 °FISO 306/B50
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 50.0 °C68.0 - 122 °FHopper
 220 - 235 °C428 - 455 °FHot Runner
Feed Temperature 200 - 215 °C392 - 419 °FInjection
Rear Barrel Temperature 215 - 230 °C419 - 446 °F
Middle Barrel Temperature 215 - 230 °C419 - 446 °F
Front Barrel Temperature 215 - 230 °C419 - 446 °F
Nozzle Temperature 215 - 230 °C419 - 446 °F
Zone 4 215 - 230 °C419 - 446 °FInjection
Melt Temperature 220 - 235 °C428 - 455 °F
Mold Temperature 20.0 - 55.0 °C68.0 - 131 °F
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6317 / 311010

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.