MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2000808D2 Silver Backlight Ink
Categories: Fluid; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Silver Ink C2000808D2 is a high resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has dark color when printed and fired on float side of glass and is fully blendable with low resistance ink C2000808D1. It can be printed onto IR or UV black enamels.

Silver Ink C2000808D2 is a grey ink with a pine smell at a ready to use viscosity suitable for firing on glass to form conductive tracks. The ink should be gently stirred before use avoiding the introduction of air bubbles.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 60 %
Particle Size <= 4.0 µmMain Break; Fineness of Grind
 <= 15 µm3rd Streak; Fineness of Grind
Viscosity 9000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT550 cone and plate viscometer (PK1.1°)
Storage Temperature <= 25.0 °C
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.016 ohmfired; 8 microns thick
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 °C
Cure Time 0.133 - 0.25 hour
Shelf Life 3.00 Month
 
Descriptive Properties
Coverage cm2/g350230 mesh stainless steel screen
Printing Mesh counts/inch180 to 340stainless steel or polyester screens

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WGEM079 / 75932

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.