MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Aflux® 12 NS Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Processing promoter for compounds based on natural and synthetic rubber

Use: Aflux 12 NS provides a good dispersion of the ingredients in the rubber compound. Mixing time can be reduced, energy savings are possible. The sticking of the compound to mixing units can be avoided. The manufacture of semifinished goods is made easier, i.e. extrusion and calendaring of heavy-filled compounds is improved. Surface structure and dimensional stability are positively influenced. Aflux 12 NS improves the flow properties of the rubber compound. Therefore it is possible to fill the molds - used for transfer and injection molding - faster and under lower pressure. Demolding of vulcanizates is facilitated.

Application: Provides processing improvement and better dispersion for technical molded and extruded goods of all kinds

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Ash 18.5 - 21.5 %
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8237 / 208630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.