AISI 8620H is a common, carburizing alloy steel used for a variety of medium-strength applications including gears, camshafts, fasteners, and chains/chain pins. Flexibility in hardening treatments allow optimization of case/core properties. Specific conditions for property data below: Normalized: heated to 915°C (1675°F), air cooled. Core properties. |
UNS H86200, AFNOR 22 NCD 2, UNI 20 NiCrMo 2, JIS SNCM 21 H, JIS SNCM 21, B.S. 805 H 20 (UK), B.S. 805 M 20 (UK), ASTM A304, SAEJ1268, DIN 1.6523, AFNOR 20 NCD 2 (France) |