MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Aremco-Bond™ 807 High Performance Epoxide
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: 10 Minute Set, Non-Sagging, 1:1, Excellent Electrical & Mechanical Properties

Vendors: Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/cc
Viscosity 75000 cP75000 cPMixed Viscosity
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7373
Shear Strength 7.826 MPa1135 psiASTM D1002-94
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm
Dielectric Constant 4.4
@Frequency 1000 Hz
4.4
@Frequency 1000 Hz
Dielectric Strength 15.0 kV/mm380 kV/in
Dissipation Factor 0.0300.030
 
Thermal PropertiesMetricEnglishComments
CTE, linear 59.0 µm/m-°C
@Temperature 20.0 °C
32.8 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 23.0 °C
1.00 hour
@Temperature 73.4 °F
Pot Life 15.0 min
@Temperature 25.0 °C
15.0 min
@Temperature 77.0 °F
100 gm mass
 
Descriptive Properties
Chemical ResistanceExcellent
ColorGray
Mix Ratio by Weight1:1resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Aremco-Bond™ 820 High Performance Epoxide
Aremco Aremco-Bond™ 657 High Performance Epoxide

PAREM06 / 24270

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.