MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Protective Coating PC-Fahrenheit™ High Temperature Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, High Temperature

Material Notes: PC-Fahrenheit™ is a hand moldable putty epoxy designed for quick emergency-type repairs formulated for increased temperatures. PC-Fahrenheit™ can be expected to outperform other putties at high temperatures. Temperatures extremes of 350°F (176°C) to 500°F (260°C) will reduce service life of the repair. High Temperatures contact may produce an objectionable odor. Cut, mix and apply. PC-Fahrenheit™ allows a working time of about 8 minutes and cures for service in 60 minutes. Example applications include mufflers and other auto uses, grills, stoves, steam pipes, etc.

Data provided by the manufacturer.

Key Words: PC Epoxy
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75751 Week Cure; ASTM D2240
Elongation at Break 1.0 %1.0 %
Compressive Yield Strength 55.16 MPa8000 psiASTM D695
Shear Strength 4.83 MPa700 psiTensile Shear Strength; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -28.9 °C-20.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourFor Service
Working Life 8.0 min
@Temperature 21.1 °C
8.0 min
@Temperature 70.0 °F
 
Descriptive Properties
ColorBrownComponent A
 BrownMixed
 KhakiComponent B
Thermal Shock ResistanceExcellent
ToxicityNontoxic after cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCOLOY® Alloy 800
Sandvik Sanicro 69 Seamless tube and pipe
Sandvik Sanicro 30 Seamless tube and pipe
Sandvik Esshete 1250 Tube and pipe, seamless
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow

PEPXP94 / 124699

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.