MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

FKuR Kunststoff Biograde® C 6530 Biodegradable Plastic Compound  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Wood and Natural Products

Material Notes: BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especially designed for injection molding applications. BIOGRADE® is mainly composed of natural resource materials (European Soft Wood from sustainable forestry) and does not contain starch or starch derivatives. Furthermore BIOGRADE® has the following advantages:
  • high content of natural resource materials
  • excellent heat resistance - up to 115 °C
  • injection mouldable on conventional injection moulding equipment
  • processable with multi-cavity moulds
  • flat sheet / film suitable for thermoforming on conventional deep drawing machinery
  • properties comparable to polystyrene: rigid and transparent depending on grade.
  • Food contact approved
  • Biodegradability certified by independent organisations.

    BIOGRADE® C 6530 is a consitent further development of BIOGRADE® C 9550. BIOGRADE® C 6530 is especially suitable for the production of injection moulded rigid parts and those with thin walls and long flow paths. This optimization are possible through the appropriate and unique combination of additives and natural fillers. Thereby it features similar characteristics as BIOGRADE® C 9550.

    Information Provided by FKuR Kunststoff GmbH
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Bulk Density 0.890 g/cc0.0322 lb/in³ISO 60
    Density 1.49 g/cc0.0538 lb/in³ISO 1183
    Melt Flow 27 - 31 g/10 min
    @Load 5.00 kg,
    Temperature 230 °C
    27 - 31 g/10 min
    @Load 11.0 lb,
    Temperature 446 °F
    ISO 1133
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength at Break 44.0 MPa6380 psiISO 527
    Tensile Strength, Yield 46.0 MPa6670 psiISO 527
    Elongation at Break 5.5 %5.5 %ISO 527
    Elongation at Yield 9.0 %9.0 %ISO 527
    Tensile Modulus 3.15 GPa457 ksiISO 527
    Flexural Yield Strength 58.0 MPa
    @Strain 3.5 %
    8410 psi
    @Strain 3.5 %
    ISO 178
    Flexural Modulus 3.00 GPa435 ksiISO 178
    Charpy Impact Unnotched 3.50 J/cm²
    @Temperature 23.0 °C
    16.7 ft-lb/in²
    @Temperature 73.4 °F
    ISO 179-1/1eU
    Charpy Impact, Notched 0.350 J/cm²
    @Temperature 23.0 °C
    1.67 ft-lb/in²
    @Temperature 73.4 °F
    ISO 179-1/1eA
     
    Thermal PropertiesMetricEnglishComments
    Melting Point >= 180 °C>= 356 °FISO 3146-C
    Vicat Softening Point 107 °C225 °FA; ISO 306
     
    Descriptive Properties
    Flexural strain at break (%)No BreakISO 178
    Melt Volume Flow (cm3/10 min)20.5-23.5ISO 1133; 230°C, 5kg

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    FKuR Kunststoff Biograde® C 6509 CL Biodegradable Plastic Compound
    FKuR Kunststoff Biograde® C 9550 Biodegradable Plastic Compound
    FKuR Kunststoff Biograde® C 7500 Biodegradable Plastic Compound
    Akzo Nobel Injection molding of 20% Wood Plastic Composite with 3.25% Expancel 092-120
    American Red Maple Wood

    PFKUR006d / 138488

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.