MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Malvern Minerals Novacite® L-337 Untreated Lamellar Quartz Filler/Extender
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automotive and industrial coatings. The unique, disc-like or lamellar shape of Novacite® makes it useful for coating systems where low oil absorption and improved barrier properties are desired. In coatings, the lamellar plate overlap parallel to the substrate surface. It has a polar, wettable surface and is very transparent in the UV and visible range. Its structure alpha (low) quartz, which is stable to 573°C. The crystallography of Novacite shows it is an uncommon variety of quartz, with anhedral or subhedral crystals that cleave along the principal axis of the molecular structure.

Information provided by Malvern Minerals Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.65 g/cc
Bulk Density 52.97 lb/ft³Loose packed
 82.75 lb/ft³Dense Packed
Brightness 80 %GE Brightness
Oil Absorption 17 - 20 %
Fineness 7.0Hegman
Water Absorption 8.7 %
 0.00 %
@Temperature 110 °C,
Time 10800 sec
 0.00 %
@Temperature 1000 °C,
Time 1800 sec
Porosity 0.50 - 0.535 %
Particle Size >= 1.0 µm13% finer
 2.0 - 3.5 µmaverage
 <= 5.0 µm79% finer
pH 6.0 - 6.3in distilled water
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 820
Hardness, Mohs 7.0
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.803 J/g-°C
@Temperature 0.000 - 200 °C
Typical Novacite; finer grades are lower than coarser grades
Transformation Temperature 573.7 °Con heating
 573.8 °Con cooling
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.550
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.102 %
CaO 0.014 %
Fe2O3 0.039 %
Loss on Ignition(%) 0.19 %
MgO 0.021 %
SiO2 99.49 %
TiO2 0.015 %
 
Descriptive Properties
Acid Number00-18
ColorGray-TanWet
 WhiteDry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives 8611 Polymer Resistor Composition

CMALV906 / 149091

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.