MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis BA11CF Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: BA110CF is a heterophasic copolymer. This grade is suitable for use on chill roll processes. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BA110CF is recommended for food packaging, lamination films, stationary films, monoaxial oriented films, and inner layer in co extrusion.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 - 0.910 g/cc0.0325 - 0.0329 lb/in³ISO 1183
Melt Flow 0.85 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.85 g/10 min
@Load 4.76 lb,
Temperature 446 °F
50% relative humidity; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 550 - 750 %550 - 750 %ISO 527-3
Film Elongation at Break, TD 550 - 750 %550 - 750 %ISO 527-3
Tensile Modulus 0.500 - 0.600 GPa72.5 - 87.0 ksiMD/TD; ISO 527-3
Flexural Modulus 1.20 GPa174 ksiISO 178
Dart Drop, Total Energy 25.0 J
@Thickness 0.0500 mm
18.4 ft-lb
@Thickness 0.00197 in
1100 N force; ISO 7765-2
Film Tensile Strength at Break, MD 40.0 - 60.0 MPa5800 - 8700 psiISO 527-3
Film Tensile Strength at Break, TD 30.0 - 50.0 MPa4350 - 7250 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 158 - 162 °C316 - 324 °F50% humidity, 23°C; ISO 3146
Vicat Softening Point 150 °C
@Load 1.02 kg
302 °F
@Load 2.25 lb
50% humidity, 23°C; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 40 %<= 40 %ASTM D1003
Gloss >= 3.0 %>= 3.0 %ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BA390TF Polypropylene Copolymer
Borealis Borcoat™ EA165E Elastomer Modified Polypropylene for Extrusion
Borealis BH374MO Polypropylene Copolymer
Overview of materials for Polypropylene, Extrusion Grade
Borealis BB213CF Polypropylene Copolymer

PBOREA301 / 108561

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.