MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Drake Plastics PAI 4435 Extruded Polyamide-Imide
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Glass Filled

Material Notes: Description: DRAKE 4435 PAI is a wear grade containing graphite, PTFE, and other additives, making it well-suited for high pressure and velocity bearings and wear parts. It offers the lowest wear rate under most non-lubricated conditions.

Typical Applications:

  • Sliding vanes
  • Thrust washers
  • Bobbins
  • Seal and piston rings

Information provided by Drake Plastics.

Vendors: Drake Plastics Ltd. Co. The Torlon Specialist, manufactures & stocks the most complete line of Torlon PAI in machinable rod, plate & Seamless Tube®. Drake works closely with Solvay Specialty Polymers to identify & serve a multitude of new applications. Drake, a lean producer of extruded, injection molded & machined shapes & parts, offers low minimums & quick, economical delivery globally.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.59 g/cc0.0574 lb/in³ASTM D792
Water Absorption 0.12 %
@Time 86400 sec
0.12 %
@Time 24.0 hour
Immersion; ASTM D570(2)
Water Absorption at Saturation 1.5 %1.5 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 6262ASTM D875
Hardness, Rockwell M 106106ASTM D875
Hardness, Shore D 8484ASTM D2240
Tensile Strength, Ultimate 90.0 MPa13100 psiASTM D638
Elongation at Break 2.00 %2.00 %ASTM D638
Tensile Modulus 3.90 GPa566 ksiASTM D638
Flexural Yield Strength 159 MPa23100 psiASTM D790
Flexural Modulus 7.59 GPa1100 ksiASTM D790
Compressive Strength 152 MPa22000 psi10% Def; ASTM D695
Compressive Modulus 6.55 GPa950 ksiASTM D695
Izod Impact, Notched 0.320 J/cm0.600 ft-lb/inType A; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C4.44 µin/in-°FASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 281 °C538 °FASTM D648
Glass Temperature Coefficient 275275ASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDRAKE80b / 326979

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.