MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TSRC T-BLEND® 2102-10T TPR/TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: T-BLEND® is a series of thermosplastic elastomer compound materials produced by TSRC (Shanghai) Industries LTD. T-BLEND® 2102-10T Can be used for plastic overmolding application, also can be used for molding directly. T-BLEND® 2102-10TCan be used Injection molding method of machining, It has weathering resistance, flexibility, ex.

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.850 - 0.890 g/cc0.850 - 0.890 g/ccASTM D792
Linear Mold Shrinkage 0.015 - 0.025 cm/cm0.015 - 0.025 in/in
Melt Flow 18 - 38 g/10 min
@Load 1.20 kg,
Temperature 120 °C
18 - 38 g/10 min
@Load 2.65 lb,
Temperature 248 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 17 - 2317 - 23ASTM D2240
Tensile Strength 0.686 MPa99.6 psiType3, specimen; ASTM D412
Elongation at Break 700 %700 %Crosshead; ASTM D412
300% Modulus 0.0981 MPa14.2 psi500mm/min; ASTM D412
Tear Strength 2.94 kN/m16.8 pliC Die; ASTM D624
 
Processing PropertiesMetricEnglishComments
Feed Temperature 150 °C302 °F
Rear Barrel Temperature 175 °C347 °F
Front Barrel Temperature 180 °C356 °F
Die Temperature 185 °C365 °F
Mold Temperature 30.0 - 40.0 °C86.0 - 104 °F
Drying Temperature 80.0 °C
@Time 3600 - 7200 sec
176 °F
@Time 1.00 - 2.00 hour
hot air circulating oven/hopper
Back Pressure 0.343 - 0.686 MPa49.7 - 99.5 psi
Cycle Time - Injection 25 - 50 sec25 - 50 sec
 
Descriptive Properties
ColorTranslucent
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTSRC053 / 306341

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.