MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Panaflex™ 945GPS Awning and Sign Facing
Categories: Polymer; Film

Material Notes: 3M™ Panaflex™ Awning and Sign Facing 945GPS is a flexible material and built-in dirt resistance on its smooth, semi-gloss surface. This durable substrate is white-pigmented vinyl with a reinforcing polyester scrim. It can be decorated first surface with 3M brand pigmented translucent film or screen or inkjet printed translucent film for use in signs and awnings. Decorated material has up to a 9-year warranted durability.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brightness 100 - 120 %100 - 120 %Whiteness
 
Optical PropertiesMetricEnglishComments
Gloss 7.5 - 27.5 %7.5 - 27.5 %
Transmission, Visible 24 - 28 %24 - 28 %
 
Descriptive Properties
Color-11.5b
 7a
 90L

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34835 / 169582

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.