Titanvene™ LL3550UA is a medium density polyethylene, which has been specially developed for manufacturing large containers. Titanvene™ LL3550UA offers excellent UV resistance (UV6) for outdoor exposure with high levels of UV light radiation where the use of inorganic pigments or carbon black is normally recommended. Applications: Titanvene™ LL3550UA is designed for large rotational molding containers, traffic cone and garbage bin. Information provided by Lotte Advanced Materials. |