Polypropylene homopolymer, extrusion coating grade, controlled rheology. Applications: - Extrusion coated paper
- Extrusion coated woven substrates
- Extrusion coated nonwoven substrates
- Other extrusion-coated applications
Information provided by Phillips Meets FDA regulation 21 CFR 177.1520 and may safely be used for articles in contact with food except for packaging or holding food during cooking.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |