MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LG Chemical LUPOY EU5000W PC/ASA, Injection Molding
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/ASA Alloy, Unreinforced

Material Notes: Weathering Resistance, Good Flow

Application: Automotive Exterior

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM D792
Melt Flow 42 g/10 min
@Load 5.00 kg,
Temperature 260 °C
42 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.9 MPa
@Thickness 3.20 mm
8110 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 50 %
@Thickness 3.20 mm
50 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Strength 76.7 MPa
@Thickness 6.40 mm
11100 psi
@Thickness 0.252 in
10mm/min; ASTM D790
Flexural Modulus 2.06 GPa
@Thickness 6.40 mm
299 ksi
@Thickness 0.252 in
10mm/min; ASTM D790
Izod Impact, Notched  0.588 J/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
1.10 ft-lb/in
@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
 1.18 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
2.20 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
@Thickness 6.40 mm
223 °F
@Thickness 0.252 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 240 - 270 °C464 - 518 °F
Middle Barrel Temperature 245 - 275 °C473 - 527 °F
Front Barrel Temperature 245 - 275 °C473 - 527 °F
Nozzle Temperature 245 - 275 °C473 - 527 °F
Melt Temperature 240 - 270 °C464 - 518 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 - 100 °C
@Time 14400 - 21600 sec
176 - 212 °F
@Time 4.00 - 6.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Back Pressure 0.490 - 1.47 MPa71.1 - 213 psi
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLHCHEM9715 / 239239

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.