MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Borealis Borcoat™ BB127E Polypropylene Adhesive Powder form for Steel Pipe Coating
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Borcoat BB127E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the Top-coat polypropylene coating Borcoat BB108E-1199.

Borcoat BB127E is delivered in powder form and can be applied with an ordinary epoxy powder gun. It has excellent adhesion to fusion bonded epoxy and polypropylene. Furthermore it has superior thermal properties and can be used at operating temperatures within the range of -10°C to 110°C, and up to 140°C for specific offshore projects.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858ISO 868
Tensile Strength, Yield 22.0 MPa3190 psiAt 50 mm/min; ISO 527-2
Elongation at Yield 6.0 %6.0 %At 50 mm/min; ISO 527-2
Tensile Modulus 1.10 GPa160 ksiAt 1 mm/min; ISO 527-2
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 108/1A
Peel Strength >= 3.00 kN/m>= 17.1 pli3-layer at 140°C; DIN 30678
 >= 4.00 kN/m>= 22.8 pli3-layer at 110°C; DIN 30678
 >= 10.0 kN/m>= 57.1 pli3-layer at 80°C; DIN 30678
 >= 20.0 kN/m>= 114 pli3-layer; DIN 30678
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 145 °C293 °FA50 (10 N); ISO 306
 
Processing PropertiesMetricEnglishComments
Front Barrel Temperature 235 - 245 °C455 - 473 °F
Head Temperature 235 - 245 °C455 - 473 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGOMER® P 121 Dispersing additive
LyondellBasell Moplen HF400G Polypropylene
LyondellBasell Moplen COAT EP/60 M BIANCO Polypropylene Copolymer
Avient Stat-Tech™ PP-16CP/000-2 HI Polypropylene
Arkema OREVAC® 18732 Grafted Maleic Anhydride Polypropylene

PBOREA044 / 27351

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.