MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Traid Villarroya TKG® FLON 15GR PTFE, 15% Graphite Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Great thermal conductivity
  • Low permeability
  • Low coefficient of friction
  • Good self-lubricant
Industry Applications:
  • Dynamic seal applications
  • Steering applications
  • Shock absorber gaskets for light and heavy duty vehicle applications

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.19 g/cc
Deformation 5.0 - 5.5 %
@Time 86400 sec
Permanent; ASTM D621
 9.5 - 11 %
@Time 86400 sec,
Pressure 13.7 MPa
ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 55
Tensile Strength >= 18.0 MPaASTM D 4894
Elongation at Break >= 200 %ASTM D 4894
Coefficient of Friction, Dynamic 0.090 - 0.11ASTM D1894
Coefficient of Friction, Static 0.12 - 0.14ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cmASTM D 257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 - 135 µm/m-°C
@Temperature 25.0 - 100 °C
ASTM D696
Maximum Service Temperature, Air 260 °CShort term
 260 °CLong term
Minimum Service Temperature, Air -200 °CShort term
 -200 °CLong term
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAID923 / 318884

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.