MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Taiwan PU Corporation TPU-E85 General Grade, Extrusion Molding Polyester Base TPU
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion Molding

Information provided by Taiwan PU Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585
Tensile Strength at Break 20.59 MPa2986 psi
Elongation at Break 900 %900 %
100% Modulus 5.40 MPa
@Strain 100 %
783 psi
@Strain 100 %
300% Modulus 8.80 MPa
@Strain 300 %
1280 psi
@Strain 300 %
Resilience 4040%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 1515
 
Processing PropertiesMetricEnglishComments
Feed Temperature 180 °C356 °F
Middle Barrel Temperature 185 °C365 °FCompress zone
Front Barrel Temperature 190 °C374 °FMetering zone
Adapter Temperature 195 °C383 °F
Die Temperature 195 °C383 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Tecoflex® EG-93A TPU - Clear
Lubrizol LifeSciences Tecoflex® EG-85A TPU - Clear
Lubrizol Estane® S190A Thermoplastic Polyurethane
Lubrizol Estane® S185A Thermoplastic Polyurethane
Lubrizol Advanced Materials Pearlstick® 45-90/03 Polycaprolactone based TPU

PTPU01 / 70857

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.