MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

MetalTek IN® 713 UNS N07713 Centri-Vac Nickel Cobalt Based Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Information provided by MetalTek

Key Words: Cast UNS N07713; AMS 5377; AMS 5391 (Investment Casting)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.91 g/cc0.286 lb/in³Based on UNS number
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 760 MPa>= 110000 psi
Tensile Strength, Yield >= 690 MPa>= 100000 psi
Elongation at Break >= 3.0 %>= 3.0 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.5 - 6.5 %5.5 - 6.5 %
Carbon, C <= 0.20 %<= 0.20 %
Cb + Ta 1.0 - 3.0 %1.0 - 3.0 %
Chromium, Cr 13 - 15 %13 - 15 %
Molybdenum, Mo 2.5 - 5.5 %2.5 - 5.5 %
Nickel, Ni 68.55 - 77.05 %68.55 - 77.05 %As Balance
Titanium, Ti 0.75 - 1.25 %0.75 - 1.25 %
 
Descriptive Properties
Heat TreatmentNot Heat Treated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alloy 713C Cast Nickel Superalloy (UNS N07713)
MetalTek IN® 718 UNS N07718 Centri-Vac Nickel Cobalt Based Alloy
Alloy 713LC Cast Nickel Superalloy
Elmet-Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
MetalTek IN® 909 Centri-Vac Nickel Cobalt Based Alloy

NMETEK151 / 18401

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.