MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kazanorgsintez Butyl Cellosolve, Industrial, Ethyleneglycolmonobutylether
Categories: Fluid; Solvent

Material Notes: Production Method: Oxyethylation

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.898 - 0.904 g/cc0.0324 - 0.0327 lb/inĀ³
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.416 - 1.4221.416 - 1.422
 
Component Elements PropertiesMetricEnglishComments
Free Water <= 0.20 %<= 0.20 %High Grade
 <= 0.25 %<= 0.25 %1st Grade
 
Descriptive Properties
Color10Hazen units, High Grade
 30Hazen units, 1st Grade
Mass Content (%)0.005Mass content of acids in conversion to acetic acid
 96.5Mass content of butyl cellosolve, 1st Grade
 99Mass content of butyl cellosolve, High Grade
Saponification Number, mg of KOH per 1 g of Butyl Cellosolve1High Grade
 1.51st Grade

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKAZAN116 / 127435

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.