MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Chase Electronic Coatings HumiSeal® UV40-250 UV Urethane Conformal Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: HumiSeal® UV40-250 is a single component, high solids, UV curable, acrylated polyurethane conformal coating that possesses excellent chemical resistance, surface hardness, flexibility and moisture resistance. The material is tack free after exposure to UV light. A secondary moisture cure mechanism will cure unexposed areas of the coating within 2-3 days at ambient conditions. The coating fluoresces under UV light to allow for coating inspection and can be applied by all selective coating equipment. HumiSeal® UV40-250 is recognized under UL File Number E105698 and is IPC-CC-830 and RoHS Directive 2011/65/EC compliant.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/cc
Solids Content >= 95 %
Viscosity 250 - 350 cPFed-Std-141, Meth. 4287
Thickness 25.0 - 125 micronsRecommended coating
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 1.06 GPa
@Temperature 60.0 °C
DMA
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 4.70e+10 ohmMoisture; MIL-I-46058C
 8.00e+14 ohmMIL-I-46058C
Dielectric Constant 2.41
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150-98
Dissipation Factor 0.010
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150-98
 
Thermal PropertiesOriginal ValueComments
CTE, linear 112 µm/m-°C
@Temperature <=26.0 °C
Below Tg; TMA
 283 µm/m-°C
@Temperature >=26.0 °C
Above Tg; TMA
Glass Transition Temp, Tg 26.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 23.0 °C
DOM
 
Descriptive Properties
Dielectric Withstand>1500 Vper MIL_I_46058C
Fungus ResistancePassesASTM G21
Resistance to ChemicalsExcellent
Thermal Shock-65 to 125°Cper MIL_I_46058C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket
Coastal Enterprises Plus™ PBHT-40 High Density Urethane Foam
Coastal Enterprises Plus™ PBHT-15 High Density Urethane Foam
CMT Materials REN Shape® 472 Machinable Board for Prototype Tooling & Assembly Fixtures
Carbon-Core CarbonFoam PU 2 R PU

PCHAS919 / 239780

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.