System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
INEOS Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Conditioned)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
;
Nylon (Polyamide PA)
Material Notes:
Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.12
g/cc
dry; ISO 1183
Moisture Absorption at Equilibrium
1.3 %
beginning dry (23°C/50% R.H.); ISO 62
Melt Flow
14
g/10 min
@Load 10.0 kg,
Temperature 240 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
31.0
MPa
0.2 in/min; ASTM Test
Tensile Strength, Ultimate
48.0
MPa
5mm/min; ISO 527
Tensile Strength, Yield
39.0
MPa
2 in/min; ASTM Test
Elongation at Break
4.0 %
5mm/min; ISO 527
8.0 %
0.2 in/min; ASTM Test
Tensile Modulus
2210
MPa
ASTM Test
2400
MPa
1mm/min; ISO 527
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+11
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+14
ohm
IEC 60093
Dielectric Constant
3.6
@Frequency 100 Hz
IEC 60250
3.6
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength
36.0
kV/mm
IEC 60243-1
Dissipation Factor
0.050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
550
V
IEC 60112
Processing Properties
Original Value
Comments
Melt Temperature
265
°C
Injection molding
Injection Velocity
65.0
mm/sec
Injection molding
Descriptive Properties
Commercial Status
Active America
Primary Processing Technique
Injection Molding
UL.UL-C
Yes
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
INEOS Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry)
INEOS Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled
Daicel CEVIAN® A2606 30% GF PA/ABS Alloy, DAM
Daicel CEVIAN® A2606 30% GF PA/ABS Alloy, Conditioned
INEOS Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Dry)
PBASF9033 / 84797
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.