MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Epaflex Epaline 780 A 15 15 TPU for Extrusion, Polyether based
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: EPALINE 700 series products are suitable for extrusion of cables, hoses, tubes, films, profiles, and belts. They are available from 75 shore A to 50 shore D, with inherently excellent resistance to hydrolysis and microbial attack, and very good flexibility at cold temperatures, thanks to their formulations based on PTMEG polyether polyols. They are manufactured in very narrow MFI/MVR ranges.

Information provided by Epaflex Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 90.090.0ISO 868
Tensile Strength 45.0 MPa6530 psiEN 12803
Elongation at Break 600 %600 %EN 12803
50% Modulus 4.00 MPa
@Strain 50.0 %
4.00 MPa
@Strain 50.0 %
EN 12803
100% Modulus 5.00 MPa
@Strain 100 %
725 psi
@Strain 100 %
EN 12803
300% Modulus 8.50 MPa
@Strain 300 %
1230 psi
@Strain 300 %
EN 12803
Tear Strength 70.0 kN/m399 pliISO 34
Abrasion 30.030.0EN 12770
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -40.0 °C-40.0 °FDMA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEPAFL907 / 325331

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.