Description: Pro-fax™ PH835 is a very high melt flow, controlled rheology polypropylene homopolymer resin designed for spunbond and continuous filament applications that require superior spinnability and finer fibers. Pro-fax™ PH835 resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients in Pro-fax™ PH835 resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Fibers Information provided by Basell. |