MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parson Adhesives PARTITE® 7310 Methacrylate Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: PARTITE 7310 is a two-component, 100% reactive structural adhesive specifically formulated for bonding thermoplastics, thermosets, metals and composite assemblies.

FEATURE:

  • Convenient 1:1 mix ratio, Non-sagging and thixotropic formulation
  • Excellent adhesion to metal surfaces such as aluminum, stainless steel, plated steel, galvanized metals, etc. without primer or chemical wipes.
  • Excellent impact, peel and shear resistance
  • Room temperature cured with extended open time.
APPLICATIONS:
  • Ideal for bonding all types of metals, PVC, Fiberglass, PBT, PPO, ABS, FRT, Polyurethane, Epoxy, Wood, RIM, Nylon, Polyesters, Acrylics, Gelcoats, Styrene, Aluminum, Stainless Steel, Cold Rolled Steel, etc.
  • Ideal for Automotive Components, Marine Assemblies, Electronics Enclosures, Appliances, Aerospace Parts, Electrical Components, Furniture, Windmill Assemblies, Exterior Sign and display, Plastic & Metal Fabrication, etc.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.05 lb/galActivator
 8.07 lb/galAdhesive
Brookfield Viscosity 40000 - 60000 cPSpindle TD 20 rpm, Adhesive
 40000 - 60000 cPSpindle TD 20 rpm, Activator
 90000 - 100000 cPMixed, Cure
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78ASTM D2240
Elongation at Break 7.0 - 18 %
Shear Strength 1500 psiABS/ABS, Substrate Failure; ASTM D1002
 1700 psiFRP/FRP, Fiber Tear; ASTM D1002
 2150 psiAluminum/ABS, Substrate Failure; ASTM D1002
 2900 psi1 month immersion in Acetic acid(10%); ASTM D1002
 3050 psi1 month immersion in Water @ 23°C; ASTM D1002
 3150 psi1 month immersion in Lubricating oil-HD30; ASTM D1002
 3150 psi1 month immersion in Water @ 90°C; ASTM D1002
 3150 psiStainless steel/Stainless steel, Cohesive Failure; ASTM D1002
 3190 psi1 month immersion in Gasoline; ASTM D1002
 3200 psi1 month immersion in Paraffin; ASTM D1002
 3250 psi1 month immersion in Xylene; ASTM D1002
 3250 psiAluminum/Aluminum, Cohesive Failure; ASTM D1002
 3450 psiEnvironmental Cycle, 30 days, Cohesive Failure; ASTM D1002
 3850 psiDIN 53283
Tensile Impact 18.0 ft-lb/in
Peel Strength 18.0 pliStainless Steel/Stainless Steel, Average; ASTM D3807
 20.0 pliStainless Steel/Stainless Steel, Initial; ASTM D3807
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -40.0 °F
Flash Point 51.0 °CAdhesive
 51.0 °CActivator
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourFull
 30.0 - 35.0 minFixture Time
Working Life 12.0 - 18.0 min
 
Descriptive Properties
ColorAmberActivator
 Off-WhiteAdhesive
Gap Filling<0.375 inCured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPARSN092 / 186535

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.