MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Raschig Group PiMC 1841 Metallic colors
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Adding metallic effect pigments to powder coatings gave rise to several application problems such as “spitting”. Synres-Almoco’s Metallic PiMC 1841 ensures easy processing and homogeneous surface quality. The PiMC 1841-series consists of some very appealing Aluminum, Bronze, Gold, Black and White metallic effect colors.

Applications for metallic colors can be found in: Sanitary products, Household appliances and Electrical- and automotive parts.

Information provided by Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 - 1.50 g/cc
Bulk Density 0.600 - 0.700 g/cc
Particle Size 10 - 25 µmD 0.1, SATP-114, Malvern method
 50 - 75 µmD 0.5, SATP-114, Malvern method
 100 - 175 µmD 0.9, SATP-114, Malvern method
Storage Temperature <= 20.0 °C
 
Mechanical PropertiesOriginal ValueComments
Abrasion <= 0.50
@Load 0.500 kg
[g] S42 paper, 500 turns; DIN 53799
 
Optical PropertiesOriginal ValueComments
Gloss 50 %20°
 75 %60°
 90 %85°
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Barbender cycle time75-115 s150°C, SATP-104
Powder stability>8 hrs30°C, SATP-128
Scratch resistance>2 NDIN 53799

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Zr 702 Zirconium

PRASCI35 / 179172

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.