MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cossa Polimeri ESTABLEND PA 1560 T8 GF ABS / Nylon 6 Blend, 30% Glass & Mineral Filled
Categories: Polymer; Thermoplastic; ABS Polymer; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.

30% glass fiber and mineral filler

Good impact strength, high chemical resistance, excellent heat resistance, high dimensional stability, low shrinkage

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cmISO 2577
Melt Flow 15 g/10 min
@Load 10.0 kg,
Temperature 240 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaISO 527
Elongation at Break 2.0 %ISO 527
Tensile Modulus 6500 MPaISO 527
Flexural Modulus 5800 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 135 °C
@Load 0.999 kg
50°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daicel CEVIAN® A2606 30% GF PA/ABS Alloy, DAM
Akro-Plastic Akromid® B3 GF 30 2 RM-D black (3424) PA 6 + ABS Dry, 30% Glass Filled
Elix Polymers Elix™ 230 G SAN Polymer Modifier
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled

PCOSSA928 / 156518

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.