MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient LubriOne™ ATH-000/10T 2S Acetal (POM) Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/ccASTM D792
Water Absorption 0.010 %
@Thickness 3.18 mm,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.010 - 0.020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 51.7 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 - 8.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2760 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPaASTM D790
Flexural Modulus 2760 MPaASTM D790
Izod Impact, Notched 53.4 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
Coefficient of Friction, Dynamic 0.37vs. Steel; ASTM D1894
Coefficient of Friction, Static 0.22vs. Steel; ASTM D1894
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 188 - 216 °C
 
Descriptive Properties
FeaturesGood Wear Resistance
 Homopolymer
 Low Friction
 Lubricated
FormsPellets
Generic NameAcetal (POM) Homopolymer
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAppliance Components
 Automotive Applications
 Bearings
 Business Equipment
 Consumer Applications
 Conveyor Parts
 Gears
 Industrial Applications
 Printer Parts
 Pulleys
 Rollers

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient LubriOne™ ATH-000/05T Acetal (POM) Homopolymer
Avient LubriOne™ ATH-05KV/000 Acetal (POM) Homopolymer
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)
Westlake Plastics Pomalux® Acetal Copolymer
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General

PH1PN9069 / 102905

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.